Reply To: How would you repair this bad blow out of wood during panel glue up?
Welcome! / Forums / General Woodworking Discussions / Woodworking Methods and Techniques / How would you repair this bad blow out of wood during panel glue up? / Reply To: How would you repair this bad blow out of wood during panel glue up?
![](https://woodworkingmasterclasses.com/wp-content/uploads/avatars/10236/e94413d8d1f55fc37944afb3a5a0d956-bpfull.jpg)
Would like to say thanks Joe.
“Issue management” is very educational. Not only have my knowledge been increased; but the design of an upcoming six feet wide side board has taken a leap forward, thanks to your photo of the back panel.
The included photo shows a repair of a tenon cut, which taught me:
1. Warming up cyanoacrylate glue facilitates its penetration into a gap.
2. Warm cyanoacrylate glue loses its rapid curing property.
3. The better half’s Babyliss must never ever again be brought into the workshop. That was made utterly clear.
[attachment file=”725419″]